Page 94 - General summary. Tensile strength per square inch of original section pounds. Elastic limit per square inch of original section do... Elongation per inch after rupture inch.. 6.
Page 148 - General summary, Tensile strength per sqnare inch of original section ................................. pounds. Elastic limit per square inch of original section .......................................... do..
Page 863 - .564. Sectional area, .25 square inch. Gauged length, 3". General summary. Tensile strength per square inch of original section pounds.
Page 375 - Sectional area, .25 square inch. Gauged length, 3". General summary. Tensile strength per square inch of original section ..... pounds.
Page 3 - SIR: I have the honor to submit, for transmission to Congress as required by law, a copy of the report of the commanding officer...
Page 794 - Marks, A B. Diameter, 1".129. Sectional area, 1 square inch. Gauged length, 10". Elongation of inch sections, ".16, ".19, ".18, ".20, ".25, ".52, ".33, ".22, ".19, ".16. Diameter at fracture, ".85. Area, .567 square inch. Contraction of area, 43.3 per cent. Appearance of fracture, silky. Opened fine cracks along surface of stem. In the fractured surface, near the circumference, in line of the fine cracks developed, was a small round spot of light colored metal.
Page 5 - The fact that a metal possesses a certain elastic iiinit, tensile strength, elongation and contraction of area when ruptured by once loading, fails to convey an adequate idea of what the same metal will do under circumstances of repeated stresses, or when these repeated stresses are applied in alternate directions. The present investigation pertains to the effects of alternate stresses in opposite directions in which the tensile and...
Page 1063 - Diameter, 1". Speed of rotation, 2,200 per minute. Length between end bearings, 33".
Page 587 - .75 from neck Character of broken surface fine silky • Applied loads per square Inch. Elongation per inch.
Page 4 - The receipts and expenditures were as follows: Amount appropriated for testing machine and testing work $15, 000.